Print Adhesion

I am having issues with print adhesion on my K2
I have cleaned the build plate, set the z to .25 and print temp for PLA to 205 yet it still pulls from the plate.

is there anything else i am missing?

thanks

I tend to print PLA at 220, bed 65, but it will vary by brand. I’ve never had to manually set my z offset. I do a heated bed level once a month - preheat the bed to 80 degrees for about 20 mins before running the level from the self check. That’s usually the only time I have to do auto level and have no issues with adhesion. You might want to slow down your first layer a bit too - I usually do first layer at 60mms.

I have done a factory reset and cleaned the bed again, testing a print now