You don't say how experienced you are in 3D printing or give any details of the setup you are using, so my comments may be way off the mark. If warping is only occurring on certain parts, maybe those with corners, try printing with a "Brim". For PLA, bed temperature is normally 60'C, and warping at the corners is often due to the corners of printed object cooling faster than the rest of the object.